Electrophoretic coating: If the electrophoretic coating does not strictly meet the requirements of various processes, such as long baking time, contamination of the tank liquid, and unqualified composition of the tank liquid. The surface of aluminum profiles is a rough foaming pinhole or a paint film with low gloss and uneven shrinkage varnish spots, and there are surface defects such as cracks on the profile surface.
Anodizing: The oxide film is easily mixed with impurities and turns yellow; The materials are easy to stick together, causing uneven oxidation color on the surface, forming a rainbow color, and causing poor product appearance; The profile and cooling bed are prone to forming black. K dots or white dots; High electrolyte temperature or prolonged electrolysis time can cause the surface of aluminum profiles. White opaque powder; During the oxidation process, if the profile decreases, it is easy to cause short circuits; If the concentration of sulfuric acid is not well controlled during alkaline corrosion, the corrosion resistance of the profile surface will decrease; The surface of the oxide film is also prone to occurrence. Blackening of ashes or appearance quality issues.
Powder coating: If the quality of the raw materials is poor and there is dust or impurities mixed in, particles will be generated on the surface of the profile; Compressed air that is not clean and mixed with oil or water can also cause shrinkage defects on the surface of aluminum profiles; Unreasonable matching can affect the physical properties and chemical resistance of aluminum profile products, such as hardness, impact resistance, and bending resistance; It can also cause poor appearance of the profile surface without powder and yellowing.